Mechanical Properties Metric English Comments
Tensile Strength at Break 20.9 MPa
3030 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R148AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 20.9 MPa
3030 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3830B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 20.9 MPa
3030 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible G92B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 20.9 MPa
3030 psi
ISO R 527
Stir SpA TP 78 GE OIL (PVC)
Application: Extrusion petrol-tight tubesInformation provided by STIR SpA
Tensile Strength at Break 20.9 MPa
3030 psi
ISO R 527
Stir SpA CT 85 ATC R (PVC)
Application: Insert with maximum transparencyInformation provided by STIR SpA
Tensile Strength at Break 20.9 MPa
3030 psi
ASTM D3759
3M Scotch® 863 Reinforced Strapping Tape
Scotch® Strapping Tape is reinforced with continuous polypropylene monofilaments. The polypropylene backing provides excellent abrasion, moisture and scuff resistance. The adhesive is specifically ..