Polymer Property : Tensile Strength at Break = 32350 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 223.0 MPa
32350 psi
ASTM D638
Polymer Resources NY66-G55 Nylon 66, 55% Glass Reinforced
Nylon 66, 55% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..