Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 35.49 MPa | 5147 psi | ASTM D1708 |
GEHR Plastics ECOGEHR® C-L Cellulose-Lignin Compound
(discontinued **) C-L is comprised of the wood components cellulose, natural fibers, lignin and fatty acids. It possesses many interesting properties that together are very similar to the natural wood. Consequently,.. |