Polymer Property : Tensile Strength at Break = 35.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.8 MPa
5190 psi
ASTM D638
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp
Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..