Mechanical Properties Metric English Comments
Tensile Strength at Break 36.8 MPa
5340 psi
ISO 527-1,2
Nanocyl PLASTICYL™ PP2001 Polypropylene with 3.2 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..
Tensile Strength at Break 36.8 MPa
5340 psi
50 mm/min; ASTM D638
Supreme Petrochem SP 246 Toughened Polystyrene
Characteristics Excellent clarity Very high toughness Deep drawability Improved thermal stabilityProcessing Extrusion ThermoformingApplications Thermoformed clear and deep draw products Rectangu..
Tensile Strength at Break 36.8 MPa
5340 psi
50 mm/min; ASTM D638
Supreme Petrochem SP 6450 High Heat Polystyrene
Characteristics High impact and modulus Very good flow properties High heat resistance & strength Available in any dark colorProcessing Injection moldingApplications Instrument enclosures Automo..
Tensile Strength at Break 36.8 MPa
5340 psi
ASTM D638
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin
Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack..
Tensile Strength at Break 36.8 MPa
5340 psi
ASTM D3759
3M 2552/Silver Damping Foils
General purpose vibration dampingInformation provided by 3M
Tensile Strength at Break 36.8 MPa
5340 psi
50 mm/min; ASTM D638
Supreme Petrochem SP EXP 31 Toughened Polystyrene
Characteristics Very high clarity & gloss High dart impact strength & good stiffness Good crease retention Good heat resistance High yield compared to PVC, APET Processing Extrusion Vacuum form..