Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 252 MPa | 36500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EC006APQ PEI LNP* Thermocomp EC006APQ is a compound based on Polyetherimide containing 30% Carbon Fiber. Added features include: Electrically Conductive, High Flow. |
|||
Tensile Strength at Break | 252 MPa | 36500 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |