Polymer Property : Tensile Strength at Break = 372 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 372 MPa
54000 psi
Mueller Alloy 3450 Leaded Brass (UNS C34500)
Used for screw machine products requiring some cold formability (i.e. crimping, knurling)Applications: The 3450 is used for screw machine applications requiring the ability to be cold formed either ..
Tensile Strength at Break 372 MPa
54000 psi
Mueller Alloy 3533 Dezincification Brass (UNS C35330)
Dezincification resistant brass suitable for high speed machining applicationsApplications: The alloy is best suitable where potential corrosion (such as dezincification) may occur. Applications fo..