Mechanical Properties Metric English Comments
Tensile Strength at Break 3800 MPa
551000 psi
ASTM D3379-94
SGL Carbon Group SIGRAFIL C® C30 S003 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3800 MPa
551000 psi
ASTM D3379-95
SGL Carbon Group SIGRAFIL C® C30 S006 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3800 MPa
551000 psi
ASTM D3379-96
SGL Carbon Group SIGRAFIL C® C30 S009 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3800 MPa
551000 psi
ASTM D3379-97
SGL Carbon Group SIGRAFIL C® C30 S012 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Tensile Strength at Break 3800 MPa
551000 psi
ASTM D3379-76
SGL Carbon Group SIGRAFIL C® C30 T045 EPY Continuous Tow Carbon Fiber with 45k filaments, Epoxy Sizing
SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes..
Tensile Strength at Break 3800 MPa
551000 psi
ASTM D3379-78
SGL Carbon Group SIGRAFIL C® C30 T400 EPY Continuous Tow Carbon Fiber with 400k filaments, Epoxy Sizing
SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes..