Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 26.5 MPa | 3850 psi | 2 in/min; ASTM D638 |
RheTech Products P250-01 Polypropylene Copolymer, Black Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 26.5 MPa | 3850 psi | 2 in/min; ASTM D638 |
RheTech Products P251-01 Polypropylene Copolymer, Black Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 26.5 MPa | 3850 psi | 2 in/min; ASTM D638 |
RheTech Products P254-01 Polypropylene Copolymer, Black Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 26.5 MPa | 3850 psi | 2 in/min; ASTM D638 |
RheTech Products P256-01 Polypropylene Copolymer, Black Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 26.5 MPa | 3850 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® M6138 High Density Polyethylene ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness... |