Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 27.2 MPa | 3940 psi | AVG; ASTM D412 Method A |
Seals Eastern 7344 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 27.2 MPa | 3940 psi | AVG; ASTM D412 Method A |
Seals Eastern 7345 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 27.1 MPa | 3940 psi | ASTM D3759 |
3M 8891 Bond Breaker Tape 3M™ Bond Breaker Tape 8891 is a black polypropylene tape that provides a unique way to break the bond of sealant between the cement joints. The tape does not allow the sealant to adhere to the tape.. |
|||
Tensile Strength at Break | 27.1 MPa | 3940 psi | ASTM D3759 |
3M Tartan™ 860 Strapping Tape The polypropylene backing of Tartan™ Strapping Tape 860 provides abrasion, moisture and scuff resistance. The adhesives is specifically formulated to provide good adhesion to metallic, plastic, fib.. |