Mechanical Properties Metric English Comments
Tensile Strength at Break 274 MPa
39700 psi
ASTM D638
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Tensile Strength at Break 274 MPa
39700 psi
ASTM D 638
SABIC Innovative Plastics LNP Verton UX06451 PPA
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength at Break 274 MPa
39700 psi
ASTM D638
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.