Mechanical Properties Metric English Comments
Tensile Strength at Break 4.49 MPa

@Temperature 23.0 °C
651 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE)
Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber..