Polymer Property : Tensile Strength at Break = 4.67 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 4.67 MPa

@Time 7200 sec
677 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1060 TPE
Product Description: StarCLEAR CLR-1060 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat..
Tensile Strength at Break 4.67 MPa
677 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 181-57W180 Thermoplastic Elastomer
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It has USP Class VI Certificate of Compliance for biocompatibility, MEM elution cytotoxicity to ..