Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.07 - 2.76 MPa | 300 - 400 psi | |
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance.. |
|||
Tensile Strength at Break | 2.07 - 2.76 MPa | 300 - 400 psi | |
Master Bond MasterSil 708FR One Part, Flame Resistant Silicone Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of .. |