Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 290 MPa | 42000 psi | Lengthwise; ASTM D638 |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
Tensile Strength at Break | 290 - 338 MPa | 42000 - 49000 psi | Wire, Temper- Hard |
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and .. |