Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.96 MPa | 430 psi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6140 NC Thermoplastic Elastomer DuraGrip® 6140NC is an enhanced bonding and adhesion grade Thermoplastic Elastomer (TPE) designed for injection molding and extrusion processes. It will bond well with polycarbonate, polycarbonate .. |