Polymer Property : Tensile Strength at Break = 44200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 305 MPa
44200 psi
ISO 527-2
PolyOne OnForce™ LFT NN-40LCF/001 Grey Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..