Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 317 - 365 MPa | 46000 - 53000 psi | Wire, Temper-Ex. Hard |
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and .. |
|||
Tensile Strength at Break | 317 MPa | 46000 psi | |
Shakespeare MX-201 PP Polypropylene Monofilament Generally good chemical resistance. Good biological resistance.Information provided by Shakespeare Company. |