Mechanical Properties Metric English Comments
Tensile Strength at Break 3.24 MPa

@Time 7200 sec
470 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7335-9000 TPE
Product Description: StarFlex P 7335-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method..