Polymer Property : Tensile Strength at Break = 5.12 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.12 MPa
742 psi
DCBP Cure
Shin-Etsu Silicones SV-14000U Silicone Rubber
SV14000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat..