Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | <= 5.70 MPa | <= 827 psi | ISO/R527 |
Polykemi AB POLYelast TPE ZS506 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
Tensile Strength at Break | 5.70 MPa | 827 psi | Across flow; ASTM D412 |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Tensile Strength at Break | 5.70 MPa | 827 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 60 A.01 TPE-S, Shore A60, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 5.70 MPa | 827 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 60 HT A.01 black TPE-S, Shore A60, black TPE-SInformation provided by BARLOG plastics GmbH. |