Polymer Property : Tensile Strength at Break = 540 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.72 MPa
540 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 281-45MED Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..
Tensile Strength at Break 3.72 MPa
540 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8291-70PA Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s..
Tensile Strength at Break 3.72 MPa
540 psi
275°F, 168 hr; ASTM D573
ExxonMobil Santoprene® 8291-85PA Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s..
Tensile Strength at Break 3.72 MPa

@Temperature 23.0 °C
540 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Tensile Strength at Break 3.72 MPa
540 psi
Heat Aged 24 hours at 600F
Malvern Minerals Sliastic 437 with 50% Novacite® Daper Quartz Filler
Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company.