Polymer Property : Tensile Strength at Break = 5406 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.27 MPa
5406 psi
Taiwan PU Corporation TPU-B95 General Grade, Blow Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation.