Tensile Strength at Break 3.90 MPa
566 psi
ISO 37
PolyOne OnFlex™ S KG 70A-3S2019 Thermoplastic Elastomer (TPE)
OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tensile Strength at Break 3.90 MPa

@Temperature 23.0 °C
566 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Tensile Strength at Break 3.90 MPa

@Temperature 23.0 °C
566 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Tensile Strength at Break 3.90 MPa
566 psi
ASTM D412
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Tensile Strength at Break 3.90 MPa
566 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 121-60M200 Thermoplastic Vulcanizate - UV Resistant
Product Description: A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated with high flow properties and excellent aesthet..