Polymer Property : Tensile Strength at Break = 5740 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.6 MPa
5740 psi
ASTM D3759
3M Scotch® 8981 Filament Tape
Scotch® Filament Tape 8981 is a high-performance packaging tape reinforced with continuous glass-yarn filaments that give the tape very high tensile strength and low stretch. The clear 3M™ Scotchp..