Tensile Strength at Break 450 - 590 MPa
65300 - 85600 psi
ThyssenKrupp PAS 380 Structural Steel for Cold Forming
This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio..