Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 591 MPa | >= 85700 psi | 8 lb. Minimum Tensile Load 0.0109 in. Diameter |
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 8 lb Information provided by Shakespeare Company. |