Mechanical Properties Metric English Comments
Tensile Strength at Break 31.0 - 41.0 MPa
4500 - 5950 psi
ASTM D638
Daikin NEOFLON M-300H PCTFE Granular Molding Powder
NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Granular powders.Processing Methods: Compression molding, extrusion.Uses: Sheets, rods, tubing.Information provided by..
Tensile Strength at Break 31.0 - 41.0 MPa
4500 - 5950 psi
ASTM D638
Daikin NEOFLON M-300P PCTFE Pellets
NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Pellets.Processing Methods: Extrusion.Uses: Rods, small parts.Information provided by Daikin Industries.
Tensile Strength at Break 31.0 - 41.0 MPa
4500 - 5950 psi
ASTM D638
Daikin NEOFLON M-400H PCTFE Granular Molding Powder
NEOFLON PCTFE M-400 series is a high molecular weight type material which is suitable for applications requiring mechanical toughness and stress crack resistance.Description:Granular powders.Process..