Mechanical Properties Metric English Comments
Tensile Strength at Break 6.58 MPa

@Temperature 23.0 °C
954 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE)
Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish..
Tensile Strength at Break 6.58 MPa

@Temperature 23.0 °C
954 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE)
Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi..
Tensile Strength at Break 6.58 MPa

@Temperature 23.0 °C
954 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Strength at Break 6.58 MPa

@Temperature 23.0 °C
954 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Strength at Break 6.58 MPa

@Temperature 23.0 °C
954 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Strength at Break 6.58 MPa

@Temperature 23.0 °C
954 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Strength at Break 6.58 MPa

@Treatment Temp. 121 °C,
Time 64800 sec
954 psi

@Treatment Temp. 250 °F,
Time 18.0 hour
in ASTM #2 Oil
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation  (discontinued **)
Elvax® 40L-03 high temperature ignition cable jacket.Information provided by DuPont.
Tensile Strength at Break 6.58 MPa

@Treatment Temp. 121 °C,
Time 64800 sec
954 psi

@Treatment Temp. 250 °F,
Time 18.0 hour
in ASTM #2 Oil
DuPont Elvax® 40L-08 High Temperature Ignition Cable Jacket Formulation  (discontinued **)
Elvax® 40L-08 high temperature ignition cable jacket.Information provided by DuPont.
Tensile Strength at Break 6.58 MPa

@Time 7200 sec
954 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7380-9000 TPE
Product Description: StarFlex P 7380-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method..