Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.86 MPa
995 psi
Taiwan PU Corporation CPU-69-A/B Mixing Ratio 100/32 Polyurethane Casting Elastomer
Compound of CPU-69-A/B with a mixing ratio of 100/32.Information provided by Taiwan PU Corporation.MatWeb has a separate entry for the unmixed A nd B components.
Tensile Strength at Break 6.86 MPa
995 psi
Shin-Etsu Silicones FE-281U Fluorosilicone Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength at Break 6.86 MPa
995 psi
Shin-Etsu Silicones KE-971U Silicone Elastomer
KE971 U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).Pr..