Polymer Property : Tensile Strength at Break = 61.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 61.3 MPa
8890 psi
ASTM D3759
3M 8991 Polyester Tape
3M™ Polyester Tape 8991 is a blue polyester tape with a silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag sea..
Tensile Strength at Break 61.3 MPa
8890 psi
ASTM D3759
3M 8991L Polyester Tape
3M™ Polyester Tape 8991L is a blue polyester tape with a silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag se..