Polymer Property : Tensile Strength at Break = 6160 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.5 MPa
6160 psi
ASTM D638
IRPC Polimaxx Polene GA3245 High Density Polyethylene
CHARACTERISTICS: HIGH TOUGHNESS, GOOD EXTRUDABILITY, EXCELLENT IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR CARRIER BAGS, GROCERY BAGS, SHOPPING BAGS, INDUSTRIAL BAGS, LINER BAGS