Tensile Strength at Break 4.27 MPa

@Temperature 23.0 °C
619 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tensile Strength at Break 4.27 MPa

@Temperature 23.0 °C
619 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..