Polymer Property : Tensile Strength at Break = 63.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 63.7 MPa
9240 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 63.7 MPa
9240 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 63.7 MPa
9240 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 63.7 MPa
9240 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 63.7 MPa
9240 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced
High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung ..
Tensile Strength at Break 63.7 MPa
9240 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced
High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung ..