Mechanical Properties Metric English Comments
Tensile Strength at Break >= 490 MPa
>= 71000 psi
Carlson 904L Austenitic Stainless Steel
General Description904L is an austenitic nickel-chromium stainless steel with molybdenum and copper additions. The elevated nickel and chromium content of 904L make it resistant to corrosion in a w..