Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 721.9 MPa | >= 104700 psi | 18.5 lb. Minimum Tensile Load 0.015 in. Diameter |
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 16 lb Low stretch, high knot strength, shock strength, abrasion resistance, superior clarity.Information provided by Shakespeare Company. |