Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 724.6 MPa | >= 105100 psi | 12.9 lb. Minimum Tensile Load 0.0125 in. Diameter |
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 12 lb Low stretch, high knot strength, shock strength, abrasion resistance, superior clarity.Information provided by Shakespeare Company. |