Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 49.9 MPa | 7240 psi | 99% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Nitric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 49.9 MPa | 7240 psi | |
Abatron AboCast 8103-28 High-Performance Dielectric Epoxy AboCast 8103-28 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h.. |
|||
Tensile Strength at Break | 49.9 MPa | 7240 psi | ASTM D638 |
Bayshore Vinyl Compounds BRC R409006/HR.WHT Injection Molding Compound BRC R409006/HR is a Type 1 / Grade 1 injection molding compound developed for hot runner applications. BRC R409006/HR meets the cell classification of 12454-B. BRC R409006/HR WHT has been designed.. |