Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.7 MPa
7350 psi
chs 2 in/min; ASTM D638
Network Polymers NPS 80-0201 Crystal Polystyrene
Description: Injection Molding Grade, High Heat ResistantInformation provided by Network Polymers Inc.