Polymer Property : Tensile Strength at Break = 74.1 MPa
Polymer Property :
Tensile Strength at Break =
74.1 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
74.1
MPa
10700
psi
GB/T 1040
Beijing Evergrow Resources MoS2 Filled Nylon
Information provided by Beijing Evergrow Resources.