Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 51.5 MPa | 7470 psi | |
Indium Corp. Indalloy® 246 95.5Sn/4.0Ag/0.5Cu Lead-Free Solder Alloy Petzow (German) prior art reference makes this alloy patent-free.Information provided by the manufacturer, Indium Corporation. |