Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.517 MPa | 75.0 psi | |
3M 12049 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tensile Strength at Break | 0.517 MPa | 75.0 psi | |
3M 12050 Black 1/2" (12.7 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tensile Strength at Break | 0.517 MPa | 75.0 psi | |
3M 12062 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tensile Strength at Break | 0.517 MPa | 75.0 psi | |
3M 12046 Black 1/16" (1.6 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tensile Strength at Break | 0.517 MPa | 75.0 psi | |
3M 12048 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tensile Strength at Break | 0.517 MPa | 75.0 psi | |
3M 12054 Black 1/4" (6.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tensile Strength at Break | 0.517 MPa | 75.0 psi | |
3M 12056 Black 3/16" (4.8 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tensile Strength at Break | >= 0.517 MPa | >= 75.0 psi | ASTM D412 |
Parker Chomerics CHO-FORM 5531 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed.. |