Mechanical Properties Metric English Comments
Tensile Strength at Break 34.5 - 75.8 MPa
5000 - 11000 psi
Compared to 300 for concrete
Abatron AboJet Structural Crack-Injection Resin
Structural crack injection resin for foundations, dikes, columns, load-bearing walls and structures. Offers strength, performance, durability, cost effectiveness and restoration instead of demoliti..