Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 51.7 MPa | 7500 psi | ASTM D638 |
Oxford Polymers Oxnilon 66-4IMP Impact Modified Nylon 66 for Injection Molding Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Strength at Break | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)& Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength at Break | 51.7 MPa | 7500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (DAM)
(discontinued **) Information provided by Entec. |
|||
Tensile Strength at Break | 51.7 MPa | 7500 psi | |
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Tensile Strength at Break | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES Plaslube® PC-50/TF/15 NAT Polycarbonate |
|||
Tensile Strength at Break | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES Plastiblend® ABS/PA 1700 B1 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength at Break | >= 51.7 MPa | >= 7500 psi | |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
Tensile Strength at Break | >= 51.7 MPa @Temperature 23.9 °C |
>= 7500 psi @Temperature 75.0 °F |
|
Master Bond UV25 One component, moderate viscosity UV curable system Product Description: Master Bond UV25 is a multi-purpose, one part UV curing system for bonding, sealing, coating and encapsulation that features excellent optical clarity, good physical properties,.. |
|||
Tensile Strength at Break | >= 51.7 MPa | >= 7500 psi | |
Master Bond EP42HT-2AO-1 Two Part, Cryogenically Serviceable Epoxy Description: Master Bond EP42HT-2AO-1 Black is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material that meets NASA low outgassing specifications. It featu.. |
|||
Tensile Strength at Break | 51.7 MPa | 7500 psi | ASTM D638 |
Americas Styrenics STYRON® 685DL High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantTypical ApplicationsFoamOPSMedicalInformation provided by AmericasStyrenics LLC. |
|||
Tensile Strength at Break | 51.7 MPa | 7500 psi | ASTM D638 |
Americas Styrenics STYRON® 665 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeFood Contact CompliantTypical ApplicationsFilmInformation provided by AmericasStyrenics LLC. |
|||
Tensile Strength at Break | 51.7 MPa | 7500 psi | ASTM D638 |
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC. |