Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 76.1 MPa | 11000 psi | ASTM D3759 |
3M 3513 Copper Foil Tape EMI/RFI shielding. UL 510 Recognized.Information provided by 3M |
|||
Tensile Strength at Break | 76.1 MPa | 11000 psi | ASTM D3759 |
3M 33516 Copper Foil Tape "Tinned," corrosion resistant. UL 510 Recognized.Information provided by 3M |