Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 783 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.40 MPa
783 psi
After oven air again 168 hrs. @ 150°C; ASTM D412
Advanced Elastomer Systems Santoprene® 8281-75 Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
Tensile Strength at Break 5.40 MPa
783 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult ..
Tensile Strength at Break 5.40 MPa
783 psi
ISO 37
Alliance Polymers Viprene™ G50A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 5.40 MPa
783 psi
ISO 37
Alliance Polymers Viprene™ G50A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 5.40 MPa
783 psi
ISO 37
Alliance Polymers Viprene™ G50D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G50D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 5.40 MPa
783 psi
ISO 37
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..