Mechanical Properties Metric English Comments
Tensile Strength at Break 54.5 MPa
7900 psi
ASTM D638
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized
High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Tensile Strength at Break 54.5 MPa
7900 psi
ASTM D638
Ravago Manufacturing Americas Hysun™ A6020 ASA+PC
Available in North America Features: Good Impact Resistance and High Heat Resistance RoHS CompliantForm: PelletsInformation provided by Ravago
Tensile Strength at Break 54.5 MPa
7900 psi
TM R050-36
Resinlab® EP750 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP750 Clear is a two part unfilled epoxy structural adhesive which ingredients are listed in the Code of Federal Regulations Title 21 175.105 (Adhesives) and 175.300 (Resinous and polymer..
Tensile Strength at Break 54.5 MPa
7900 psi
ASTM D638
Polymer Resources PC/TP-GP1 PC/Polyester Alloy
High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol..
Tensile Strength at Break 54.5 MPa
7900 psi
ASTM D638
Techmer ES HiFill® TPU 85A 0152 S1
Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc.
Tensile Strength at Break 54.5 MPa
7900 psi
ASTM D638
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin
Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu..
Tensile Strength at Break 54.5 MPa
7900 psi
Abatron AboCast 8503-3/AboCure 8503-3 Colorless Epoxy
AboCast 8503-3/AboCure 8503-3 is a general purpose, medium speed, colorless epoxy casting compound with low viscosity. It has a good balance of properties with a fairly fast hardening. Suggested Use..
Tensile Strength at Break 54.5 MPa
7900 psi
ASTM D638
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..