Polymer Property : Tensile Strength at Break = 8.30 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.30 MPa
1200 psi
500mm/min; ASTM D638 Type IV Specimen
Westlake EC4056AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC4056 is a natural low density material with an 80 melt index.FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All in..
Tensile Strength at Break 8.30 MPa
1200 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 691-73W175 Thermoplastic Vulcanizate
Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for thin wall, architectural glazing and sealing applic..