Polymer Property : Tensile Strength at Break = 8.60 MPa
Polymer Property :
Tensile Strength at Break =
8.60 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
8.60
MPa
1250
psi
ISO R 527
Stir SpA Z 2000 DR AT MOD (PVC)
Application: Foamed intersoleInformation provided by STIR SpA