Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 80.5 MPa | 11700 psi | ASTM D3759 |
3M 8555 High Temperature Nylon Tape 3M™ High Temperature Nylon Tape 8555 is a 5 mil film with a non-silicone rubber adhesive that can be used to help remove thick flash during composite bonding.Information provided by 3M |